Schadensanalyse an Profilwalzen aus Siliziumnitrid

Translated title of the contribution: Schadensanalyse an Profilwalzen aus Siliziumnitrid

Walter Harrer, Roger Morrell, Robert Danzer, Karl Berroth

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Translated title of the contributionSchadensanalyse an Profilwalzen aus Siliziumnitrid
Original languageGerman
Title of host publication9. Tagung Gefüge und Bruch
PagesP18-P18