Translated title of the contribution | Nanoindentation investigations on a high pressure torsion deformed tungsten-copper composite |
---|---|
Original language | English |
Title of host publication | Proceedings of 1st Vienna Conference Micro- and Nano-Technology |
Publisher | Österreichische Tribologische Gesellschaft |
Pages | 159-166 |
Publication status | Published - 2005 |
Nanoindentation investigations on a high pressure torsion deformed tungsten-copper composite
Thomas Schöberl, I. Sabirov, Reinhard Pippan
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution