Metallographic Documentation of the Degradation of Iron and Nickel Based Alloys in HCl and H2S Containing Environments, between 480 – 680 °C

Alexander Schmid, Gregor Karl Mori, Roland Haubner

Research output: Contribution to journalArticleResearchpeer-review