Galvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91

Gerhard Gerstmayr, Gregor Mori, Wilfried Eichlseder

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Translated title of the contributionGalvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91
Original languageEnglish
Title of host publicationMagnesium Technology 2010
Pages145-150
Publication statusPublished - 2010

Cite this