Translated title of the contribution | Discrete dislocation simulation of nanoindentation: the influence of obstacles and a limited number of dislocation sources |
---|---|
Original language | English |
Pages (from-to) | 3301-3319 |
Journal | Philosophical magazine |
Volume | 28 |
Publication status | Published - 2005 |
Discrete dislocation simulation of nanoindentation: the influence of obstacles and a limited number of dislocation sources
H. G. M. Kreuzer, Reinhard Pippan
Research output: Contribution to journal › Article › Research › peer-review