Discrete dislocation simulation of nanoindentation: The effect of statistically distributed dislocations

H. G. M. Kreuzer, Reinhard Pippan

Research output: Contribution to journalArticleResearchpeer-review

12 Citations (Scopus)
Translated title of the contributionDiscrete dislocation simulation of nanoindentation: The effect of statistically distributed dislocations
Original languageEnglish
Pages (from-to)460-462
JournalMaterials science and engineering: A, Structural materials: properties, microstructure and processing
Volume400-401
DOIs
Publication statusPublished - 2005