AFM nanoindentation of pulp fibers and thin cellulose films at varying relative humidity

Christian Ganser, Ulrich Hirn, Sebastian Rohm, Robert Schennach, Christian Teichert

Research output: Contribution to journalArticleResearchpeer-review

37 Citations (Scopus)
Translated title of the contributionAFM nanoindentation of pulp fibers and thin cellulose films at varying relative humidity
Original languageEnglish
Pages (from-to)53-60
JournalHolzforschung : international journal of the biology, chemistry, physics and technology of wood
Volume68