Determining Eutectic Grain Size and Casting Defects in an Al-12Si0.8Cu-0.5Fe-0.9Mg-0.7Ni-0.2Zn Alloy

Activity: Talk or presentation Oral presentation

PeriodFeb 2017 → …
Event titleTMS 2017: 146th Annual Meeting & Exhibition
Event typeConference
LocationSan Diego, CA, United StatesShow on map