@article{0452b96c170546bf9bbdd00974f57f86,
title = "Nanoindentation testing as a powerful screening tool for assessing phase stability of nanocrystalline high-entropy alloys",
keywords = "Nanoindentation, High-entropy alloys, Severe plastic deformation, High-pressure torsion, Phase stability, Nanocrystalline",
author = "Verena Maier-Kiener and Benjamin Schuh and Easo George and Helmut Clemens and Anton Hohenwarter",
year = "2017",
doi = "http://dx.doi.org/10.1016/j.matdes.2016.11.055",
language = "English",
volume = "115",
pages = "479--485",
journal = "Materials and Design",
issn = "1873-4197 ",
publisher = "Elsevier",
}