@article{fc6f32196d4546418f39adb8817437d9,
title = "Differential Scanning Calorimetry and Thermodynamic Predictions—A Comparative Study of Al-Zn-Mg-Cu Alloys",
keywords = "aluminium alloys, Al-Zn-Mg-Cu alloys, CALPHAD, Differential scanning calorimetry",
author = "Gernot Kolb and Stefanie Scheiber and Helmut Antrekowitsch and Uggowitzer, {Peter J.} and Daniel P{\"o}schmann and Stefan Pogatscher",
year = "2016",
month = aug,
day = "3",
language = "English",
volume = "6",
journal = "Metals : open access journal ",
issn = "2075-4701",
publisher = "Multidisciplinary Digital Publishing Institute (MDPI)",
number = "8",
}